Corona (lnner) | ≥38 mN/m |
Corona (Outer) | / |
Heatshrinkage (MD) | ≤4% |
Heatshrinkage (TD) | ≤2% |
Tensile Strength (MD) | ≥120 MPa |
Tensile Strength (TD) | ≥200 MPa |
Elongation (MD) | ≤180% |
Elongation (TD) | ≤65% |
COF (Inner) | ≤0.8% |
COF (Outer) | ≤0.8% |
Haze | ≤0.3% |
Transmittance | ≥85% |
Glossiness | ≥90% |